Mechanical properties of MWPECVD diamond coatings on Si substrate via nanoindentation

Authors: Nitti M.A., Cicala G., Brescia R., Romeo A., Guion J.B., Perna G., Capozzi V.
Years: 2011
Source Title: Diamond and Related Materials
Doi: 10.1016/j.diamond.2010.12.002
Venue: P.LAS.M.I. Lab @ Bari